The primary reason for the anti-corrosion of the chimney is that rainwater enters the bottom layer along the joints or cracks. Under the effect of the traffic load, the powder and fine materials of the bottom layer are squeezed out together with the water, so that the foundation gradually loses the support ability, and finally the concrete panel cracks.
The reasons for the occurrence of the wrong disease are:
(1) The anti-corrosion disease of the chimney is not timely or improperly handled, and the roadbed fine materials move and accumulate to the rear plate under the effect of suction, forming a staggered appearance with low front plate and high rear plate;
(2) The uneven settlement of the foundation causes the two sides of the seam to form steps.
Subsidence is generally caused by the settlement or consolidation of subgrade soil, especially near bridges and culvert structures or widened roads, and some subsidence tends to occur due to lack of compaction.
The arching performance is that the plates at the joints are arching upwards, and the plates on both sides of the transverse joints are raised significantly. The primary cause of seizures is:
(1) The expansion joint is blocked by sand, stone and debris, which hinders the expansion and expansion of the board;
(2) The horizontal and straight error of the force-transmitting rod set in the expansion joint is large, which hinders the expansion and expansion of the board;
(3) Long-expanded jointed concrete slabs are prone to longitudinal instability in small bends, steep slopes and when the thickness is thin, causing arch expansion;
(4) Because of the presence of quicklime and unstable waste residue in the bottom layer, it reacts and causes the road to bulge.
1.3 Analysis of the causes of joint damage diseases
Joint hazard diseases are generally manifested as the cracking or brokenness of the marginal concrete of the slab within the width of 50 cm on both sides of the longitudinal and longitudinal joints of the cement concrete pavement. The reasons for this appearance are:
(1) The expansion joint is blocked by mud, sand, gravel and other debris, or the force transmission rod is not set properly, which prevents the thermal expansion of the plate, and excessive temperature stress causes the edge of the plate to burst;
(2) The shrinkage joints make the concrete slabs form a void surface, and the quality of the joint filler cannot be guaranteed, so that the edges of the slabs are crushed under the repeated effects of wheel loads;
(3) Because the cutting time is too early, the seam edge is damaged earlier and damaged in the future;
(4) Poor quality of joint filler, such as low bonding strength, poor elongation and elasticity, not resistant to aging, and unreliable bonding of joint filler and joint wall.